Abstract
A thick Al2O3 film is inserted as a pre-deposited layer to overlay the transition region on bare BK7 in atomic layer deposition. The average reflectance is 0.535% (400~680nm) in practice, compared with the designed 0.408%.
© 2013 Optical Society of America