Combined Advanced Finishing and UV-Laser Conditioning for Producing UV-Damage-Resistant Fused Silica Optics

Not Accessible

Your library or personal account may give you access

Abstract

During the past year, we have focused on optimizing the laser damage performance for fused silica optics at 355-nm, 3-nsec pulse length, via application of magnetorheological finishing (MRF), wet chemical etching, and UV laser conditioning.

© 2002 Optical Society of America

PDF Article
More Like This
Experiments on Magnetorheological Finishing of Optical Polymers

Jessica E. DeGroote, Stephen D. Jacobs, and John M. Schoen
OMB1 Optical Fabrication and Testing (OF&T) 2002

Novel Approach in Magnetorheological Finishing (MRF) System Configuration

William Kordonski, Don Golini, Stephen Hogan, and Andy Price
OMA1 Optical Fabrication and Testing (OF&T) 2002

Select as filters


Select Topics Cancel
© Copyright 2024 | Optica Publishing Group. All rights reserved, including rights for text and data mining and training of artificial technologies or similar technologies.