By chelate precursor doping technique, a 30μm-core Yb-doped aluminophosphosilicate fiber was fabricated and presented 6.03kW laser output at 1080nm. The slope efficiency is 68.37% and the M2 factor is ~2.38 when stably running at 5.16kW.

© 2017 Optical Society of America

PDF Article
More Like This
KW-level Yb-doped Aluminophosphosilicate Fiber by Chelate Precursor Doping Technique

Yuying Wang, Huan Zhan, Cong Gao, Kun Peng, Zhaonian Jia, Zhen Wang, Li Ni, Xiaolong Wang, Jianjun Wang, Feng Jing, and Aoxiang Lin
ATu3K.6 CLEO: Applications and Technology (CLEO:A&T) 2016

Yb-doped LMA fiber fabrication using chelate precursor doping technique

Zhen Wang, Cong Gao, Li Ni, Xiaolong Wang, Kun Peng, Yuying Wang, Huan Zhan, Jianjun Wang, Feng Jing, and Aoxiang Lin
25B2_2 Conference on Lasers and Electro-Optics/Pacific Rim (CLEO/PR) 2015

KW-level Yb/Ce-codoped Aluminosilicate Fiber Fabricated by Chelate Precursor Doping Technique

Yuwei Li, Huan Zhan, Yuying Wang, Kun Peng, Shuang Liu, Xiaolong Wang, Li Ni, Shihao Sun, Jiali Jiang, Lei Jiang, Juan Yu, Jianjun Wang, Feng Jing, and Aoxiang Lin
JTh2A.91 CLEO: Applications and Technology (CLEO:A&T) 2018

Select as filters


Select Topics Cancel
© Copyright 2024 | Optica Publishing Group. All rights reserved, including rights for text and data mining and training of artificial technologies or similar technologies.