New Hydrogen Aging Loss Mechanism in the 1400 nm Window

Not Accessible

Your library or personal account may give you access

Abstract

A new type of hydrogen aging loss increase of up to 0.21 dB/km at the 1385 nm OH peak can arise in some fibers when exposed to 0.01 atmospheres of hydrogen for less than 4 days at room-temperature.

© 1999 Optical Society of America

PDF Article
More Like This
Alkali Impurities and the Long-Wavelength Hydrogen-Induced Aging Loss in Ge-Doped Silica Fibers

Kai H. Chang
OThQ3 Optical Fiber Communication Conference (OFC) 2005

Mechanisms of hydrogen-induced losses in silica based optical fibers

A. IINO, M. KUWABARA, and Y. MATSUDA
TUB3 Optical Fiber Communication Conference (OFC) 1990

Stability of the UV-Induced Index Change in Hydrogen-Loaded Fibers

Victor Grubsky, Dmitry S. Starodubov, and Jack Feinberg
270 Wavelength Division Multiplexing Components (WDM) 1999

Select as filters


Select Topics Cancel
© Copyright 2024 | Optica Publishing Group. All rights reserved, including rights for text and data mining and training of artificial technologies or similar technologies.