Abstract
Transmittance exceeding 92 %m-1 at 266 nm and its permanence after 4 G pulses of laser irradiation are realized in fluorine-doped silica fiber due to the optimized fiber-manufacturing processes such as perform-fabrication and fiber-drawing.
© 2008 Optical Society of America