Abstract
Using laser heated pedestal method to grow CaO or MgO side deposited Cr4+:YAG crystal fiber, Cr4+ concentration was raised by a factor of 110% after re-growth and annealing at 1350 oC in Ca,Cr:YAG crystal fiber.
© 2008 Optical Society of America