Abstract
An air-core, 252 holes cladding, 51% air-occupied fraction PMMA-based MPOF as successfully fabricated by drawing an extruded 253 holes preform. With the extrusion technique, air-core MPOF preform could be produced on a large scale.
© 2008 Optical Society of America