Abstract
Nd3+: SrWO4 crystal was pumped by alexandrite laser radiation. Raman self-conversion at 1170 nm was achieved in Q-switched (by LiF:F2- crystal) or mode-locked (by ML51 or 3955 saturable absorber) regime. Yellow emission at 585 nm (SHG) was reached.
© 2004 Optical Society of America
PDF ArticleMore Like This
J. Šulc, H. Jelínková, P. Černý, M. Doroschenko, V. V. Skornyakov, S. B. Kravtsov, T. T. Basiev, and P. G. Zverev
308 Advanced Solid-State Photonics (ASSL) 2004
Tasoltan T. Basiev, Peter G. Zverev, Alexander Ya. Karasik, Sergey V. Vassiliev, Alexander A. Sobol, Dmitri S. Chunaev, Vasily A. Konjushkin, Alexander I. Zagumennyi, Yuri D. Zavartsev, Sergey A. Kutovoi, Vyacheslav V. Osiko, and Ivan A. Shcherbakov
298 Advanced Solid-State Photonics (ASSL) 2004
Tasoltan T. Basiev, Yuri K. Danileiko, Maxim E. Doroshenko, Vyacheslav V. Osiko, Alexander V. Fedin, Andrey V. Gavrilov, and Sergey N. Smetanin